Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 50

@Time 15.0 sec
50

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 2.50 MPa
<= 363 psi
ISO/R527
Elongation at Break 700 %
700 %
ISO/R527
100% Modulus 0.00120 GPa
0.174 ksi
ISO/R527
300% Modulus 0.00160 GPa
0.232 ksi
ISO/R527
Compression Set 25 %

@Temperature 23.0 °C,
Time 259000 sec
25 %

@Temperature 73.4 °F,
Time 72.0 hour
DIN 53517
92 %

@Temperature 70.0 °C,
Time 86400 sec
92 %

@Temperature 158 °F,
Time 24.0 hour
DIN 53517
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Descriptive Properties Value Comments
Holding Pressure () Low
% of injection pressure
Injection Pressure Low
Injection Speed () High