Polyram Polytron A60N02 Nylon 66, Chemically Coupled 60% Long Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 60% Glass Fiber Filled
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron A60N02 Nylon 66, Chemically Coupled 60% Long Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A CHEMICALLY COUPLED 60% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 285 MPa
41300 psi
ASTM-D638
Elongation at Break 1.6 %
1.6 %
ASTM-D638
Tensile Modulus 21.5 GPa
3120 ksi
ASTM-D790
Flexural Strength 455 MPa
66000 psi
ASTM-D790
Flexural Modulus 19.4 GPa
2810 ksi
ASTM-D790
Izod Impact, Notched 5.50 J/cm

@Temperature 23.0 °C
10.3 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
ASTM-D648