Polyram RamOfin PPH302G6 Polypropylene, 30% Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPH302G6 Polypropylene, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ASTM-D638
Elongation at Break 2.5 %
2.5 %
ASTM-D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 5.60 GPa
812 ksi
ASTM-D790
Izod Impact, Notched 0.850 J/cm

@Temperature 23.0 °C
1.59 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
140 °C
284 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 153 °C
307 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in