Premix Thermoplastics PREBLACK PP 704-35 Polypropylene, 35% Carbon Black

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with Carbon Black Filler
Manufacturer Premix Thermoplastics Inc.
Trade Name PREBLACK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PREBLACK PP 704-35 Polypropylene, 35% Carbon Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene based PREBLACK PP 704-35 black colour concentrate has been developed especially for the colouring of polypropylene fibres. Due to its excellent homogeneity and suitable flow characteristics PREBLACK PP 704-35 is recommended for demanding fibre applications, such as CF, POY and BCF-yarns. PREBLACK PP 704-35 can also be used for tinting. According to BgVV regulations PREBLACK PP 704-35 is approved for use in contact with foodstuffs as long as the content of carbon black in the produced product is less than 2.5%. Dosing .5-10% depending on desired blackness.Information from Premix OY
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
when produced
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Colour Brownish
Light Fastness 8
Very Good