Material Notes:
BUNA-N should be considered for use with oils and animal fats. This is a food grade and 3A approved that has good compression set characteristics. BUNA-N does have a limited temperature range which precludes its use in many applications. This material does not meet USP Class VI.Information provided by Process Technologies Inc
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.33 °C
200.0 °F
Minimum Service Temperature, Air -34.44 °C
-29.99 °F
Descriptive Properties Value Comments
Color Black
Blue
Green
Red
White
Yellow
Compatibility for Chemicals Acetone
Not Recommended
Ammonia
Good
Hydrochloric Acid
Not Recommended
Hydrofluoric Acid
Not Recommended
Hydrogen Peroxide
Good
Isopropyl Alcohol
Good
Nitric Acid
Not Recommended
Phosphoric Acid
Good
Sodium Hydroxide
Good
Sodium Hypochlorite
Good
Steam to 400ºF (204ºC)
Not Recommended
Sulfuric Acid
Limited