Pyrotek Bonded Particle Filtration Media

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Bonded Particle Filtration Media.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bonded particle filtration media is a proven and efficient means for removing oxides from molten aluminum and its alloys. This filtration media is available in either high strength alumina oxide or silicon carbide, and can be supplied in plate, cylindrical and custom shapes. ApplicationsIn-line filtration (filter wall) Dip wells Charge wells Stalk Tubes AdvantagesImproves Melt Quality Stronger than ceramic foam filters Easy to install Long service life Thermally conductive Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1093 °C
1999 °F