Pyrotek Fiberseal Paper C-3 Ceramic fiber paper

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name Fiberseal Paper
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Fiberseal Paper C-3 Ceramic fiber paper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C-3 fiberseal paper is designed for applications where high temperature protection is required. C-3 is resistant to most chemicals with exception of hydrofluoric and phosphoric acids and strong alkalis.ApplicationsIndustrial gaskets Liquid metal back-up insulation Brazing furnace insulation Investment casting parting agent AdvantagesResistant to most chemicals Thermal properties remain unaffected by exposure to water or steam Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.192 - 0.224 g/cc
0.00694 - 0.00809 lb/in³
Binder 0.080 - 0.14
0.080 - 0.14
organic
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1260 °C
2300 °F
Component Elements Properties Metric English Comments
Al2O3 50 %
50 %
SiO2 48 %
48 %