Pyrotek M-1 High-Temperature Felt

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek M-1 High-Temperature Felt.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A light-brown material.Dimensions483 mm x 7.6 m 13 mm thickApplicationsHigh-temperature gasketsInformation provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.0480 g/cc
0.00173 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1260 °C
2300 °F