Pyrotek PROSILY G-42A Graphite Lubricant/Coating

Category Carbon , Graphite
Manufacturer Pyrotek, Inc.
Trade Name PROSILY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek PROSILY G-42A Graphite Lubricant/Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color - Black, Base - Graphite, Carrier - AerosolApplicationsGraphite spray Coating lubricator AdvantagesResistant to high temperature Good thermal conductivity Low coefficient of expansion Chemically inert Information provided by Pyrotek.
Physical Properties Metric English Comments
Solids Content 22 %
22 %