Pyrocast FSC-2000 eliminates the need for cement pre-mixing or rolling while providing the same outstanding characteristics of all dense fused silica products.ApplicationsAdhesive Coating Patching compound for refractory shapes Joining compound for fused silica foam Facing compound for fused silica foam AdvantagesErosion resistant Resistant to thermal shock Retains strength at elevated temperatures Extremely low co-efficient of thermal expansion Aids skull removal Reduces erosion on metal surfaces Requires minimal pre-mixing or rolling Freeze protected Easily applied Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.698 - 1.794 g/cc
0.06134 - 0.06481 lb/in³
Porosity 20 - 24 %
20 - 24 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00300 GPa
0.435 ksi
Compressive Strength 83.0 MPa
12000 psi
Thermal Properties Metric English Comments
Flash Point >= 2038 °C
>= 3700 °F