Pyrotek Pyrocast XL Small Component Refractory

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name Pyrocast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyrocast XL Small Component Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast surface Dimensionally stable Preheating unnecessary Easily cleaned Non-wetting Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.90 - 1.95 g/cc
0.0686 - 0.0704 lb/in³
Open Porosity 22 - 23 %
22 - 23 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0140 GPa

@Treatment Temp. 725 °C
2.03 ksi

@Treatment Temp. 1340 °F
Compressive Strength 55.0 MPa
7980 psi
cured at 725°C
Thermal Properties Metric English Comments
CTE, linear 0.820 µm/m-°C

@Temperature 200 - 700 °C
0.456 µin/in-°F

@Temperature 392 - 1290 °F
Thermal Conductivity 0.860 W/m-K

@Temperature 460 °C
5.97 BTU-in/hr-ft²-°F

@Temperature 860 °F
0.880 W/m-K

@Temperature 610 °C
6.11 BTU-in/hr-ft²-°F

@Temperature 1130 °F
0.930 W/m-K

@Temperature 790 °C
6.45 BTU-in/hr-ft²-°F

@Temperature 1450 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Shrinkage -0.0770 %

@Temperature 700 °C
-0.0770 %

@Temperature 1290 °F
Linear
Component Elements Properties Metric English Comments
Al2O3 36.7 %
36.7 %
CaO 6.3 %
6.3 %
Other 3.0 %
3.0 %
SiO2 54 %
54 %