Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Heraflex® A 90-11-44 UV TPS-SEBS Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Radici Group Plastics
Trade Name Heraflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Heraflex® A 90-11-44 UV TPS-SEBS Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPS-SEBS Thermoplastic Elastomer. 92 Shore A, low odor level and stable to light. Scratch resistance, dry grip.Application examples: Cover for hand brake leverProcessing technology: Injection moldingSpecial properties: Weather resistantInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90