Ravago Manufacturing Americas Enviramid™ N2320HL BK Post Consumer Recycle Nylon 6, 20% Glass Filled

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Enviramid™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Enviramid™ N2320HL BK Post Consumer Recycle Nylon 6, 20% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Water Absorption 1.3 %
1.3 %
Saturation, Immersed; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 163 MPa
23600 psi
ASTM D790
Flexural Modulus 4.800 GPa
696.2 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
ASTM D648