Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylex® P1010G20FRMA Polycarbonate, 20% Glass Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylex® P1010G20FRMA Polycarbonate, 20% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate, 20% Glass Filled, Flame RetardantInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm

@Thickness 3.17 mm
0.0020 - 0.0050 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 135 MPa
19600 psi
ASTM D790
Flexural Modulus 5.500 GPa
797.7 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D785
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648
Vicat Softening Point 166 °C
330 °F
ASTM D1525
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0 - 5VA

@Thickness 3.00 mm
V-0 - 5VA

@Thickness 0.118 in
Users viewing this material also viewed the following: