Ravago Manufacturing Americas Hylex® P1332L Polycarbonate, UV Stabilized, Unreinforced

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylex® P1332L Polycarbonate, UV Stabilized, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
24-Hr Immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 32 g/10 min

@Load 1.20 kg,
Temperature 300 °C
32 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Tensile Strength, Yield 66.9 MPa
9700 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Flexural Strength 86.2 MPa
12500 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
0.988 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
1.85 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
259 °F
ASTM D648
Vicat Softening Point 152 °C
305 °F
ASTM D1525
Flammability, UL94 V-2
V-2
0.059 inches
Optical Properties Metric English Comments
Refractive Index 1.585
1.585
ASTM D542
Haze 0.50 - 0.80 %

@Thickness 3.17 mm
0.50 - 0.80 %

@Thickness 0.125 in
ASTM D1003
Transmission, Visible 89 - 91 %

@Thickness 3.17 mm
89 - 91 %

@Thickness 0.125 in
Electrical Properties Metric English Comments
Electrical Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Dielectric Strength 16.0 kV/mm

@Thickness 3.17 mm
406 kV/in

@Thickness 0.125 in
in Air; ASTM D149
Arc Resistance 120 sec
120 sec
ASTM D495