Material Notes:
Description: Produced by thermal processes. Used in wear parts, engine and machine components, mill media, refractories, ceramic pigments. fuel cells, laser, and capacitors.Forms Available: Various granulations are available down to nanosize.Information provided by Reade Advanced Materials.
Physical Properties Metric English Comments
Specific Gravity 5.75 g/cc
5.75 g/cc
Density 5.700 g/cc
0.2059 lb/in³
Molecular Weight 123.22 g/mol
123.22 g/mol
Mechanical Properties Metric English Comments
Hardness, Mohs 6.5
6.5
20°C
Thermal Properties Metric English Comments
Melting Point 2700 °C
4890 °F
Boiling Point 5500 °C
9930 °F
Descriptive Properties Value Comments
Color gray black
Crystal Structure monoclinic