Reade Advanced Materials Diatomite Powder

Category Ceramic
Manufacturer Reade Advanced Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reade Advanced Materials Diatomite Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Diatomite is a sedimentary rock, white to light yellow in color, composed of the fossilized skeletons of diatoms, one celled algae-like plants which accumulated in marine or lacustrine environments. The honeycomb silica structures gives diatomite useful characteristics such as high absorptive capacity and surface area, chemical stability, and low bulk density.Diatomite is principally used in filtration of various alcoholic beverages, sugar, oil, organic and inorganic chemicals, and water. It is also used as a filler in absorbents for pet litter and oil spills. Other uses are: pesticide carrier, roughness and flatting agent in paint; an anti-blocking agent in polyethylene film; a soft abrasive in silver and automotive polishes; or as bulk extender. Small amounts of diatomite are used as a thermal insulator and catalyst carrier.Form Available: Fine grained powderInformation provided by Reade Advanced Materials.
Physical Properties Metric English Comments
Specific Gravity 2.10 g/cc
2.10 g/cc
pH <= 7.0
<= 7.0
Optical Properties Metric English Comments
Refractive Index 1.43
1.43
Descriptive Properties Value Comments
Color buff white