Reliance Industries Repol B220MN Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol B220MN Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REPOL Polypropylene B220MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol B220MN is recommended for use in injection molding processes where high flow and medium impact strength are required. It is an ideal material for rigid packaging, automotive components, housewares and appliances parts. Repol B220MN contains nucleating agent. Features:Excellent flow characteristics Short molding cycleConsistent processabilityGood stiffness-impact balanceGood surface glossInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
50mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
50mm/min; ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.700 J/cm

@Temperature 23.0 °C
1.31 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648