Material Notes:
REPOL Polypropylene H030SG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H030SG is recommended for Raffia Tapes used in making woven fabrics for sacking, carpet backing, industrial packaging and geotextile applications.Features:High tenacity in tapesConsistent processabilityLow "water carryover"Good color and processing stabilityInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
50mm/min; ASTM D638
Elongation at Yield 10 %
10 %
50mm/min; ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648