Resin Technology Group 24N Two component Polyurethane Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group 24N Two component Polyurethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Technology Group 24N Two component Polyurethane AdhesiveHigh impact, polycarbonate and PVC bonding urethane
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 90
80 - 90
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Gel Time 5.00 - 10.0 min
5.00 - 10.0 min
Descriptive Properties Value Comments
Color Black