Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP LCL36 PEEK (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP LCL36 PEEK (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* LCL36 is a compound based on Polyetheretherketone containing Carbon Fiber , PTFE. Added features of this material include Electrically Conductive, Internally Lubricated.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 201 MPa
29200 psi
5 mm/min; ISO 527
Elongation at Break 3.7 %
3.7 %
5 mm/min; ISO 527
Tensile Modulus 13.5 GPa
1960 ksi
1 mm/min; ISO 527
Flexural Strength 267 MPa
38700 psi
2 mm/min; ISO 178
Flexural Modulus 16.3 GPa
2360 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 300 °C
>= 572 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 0.700 mm
V-0

@Thickness 0.0276 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257