Material Notes:
LNP* Lubricomp* PFL-4216 is a compound based on Nylon 6 resin containing Glass Fiber, MOS2. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 168 MPa
24400 psi
ASTM D638
Elongation at Break 3.3 %
3.3 %
ASTM D638
Tensile Modulus 9.90 GPa
1440 ksi
50 mm/min; ASTM D638
Flexural Strength 248 MPa
36000 psi
ASTM D790
Flexural Modulus 8.70 GPa
1260 ksi
ASTM D790
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.81 J/cm
22.12 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D648