SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* RA004 is a compound based on Nylon 66 resin containing 20% Aramid. Added features of this material include: Wear Resistant.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.015 cm/cm

@Time 86400 sec
0.015 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 88.0 MPa
12800 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 137 MPa
19900 psi
ASTM D790
Flexural Modulus 4.41 GPa
640 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.68 J/cm
6.89 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 171 °C

@Thickness 3.20 mm
340 °F

@Thickness 0.126 in
unannealed; ASTM D648