SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT (Asia Pacific)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* WX95752L is a compound based on Polybutylene Terephalate resin. Added features of this material include: Internally Lubricated, Low Extractible.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.030 cm/cm

@Time 86400 sec
0.030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 30.6 %
30.6 %
ASTM D638
Tensile Modulus 2.40 GPa
348 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 13.69 J/cm
25.65 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C

@Thickness 3.20 mm
131 °F

@Thickness 0.126 in
unannealed; ASTM D648