Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Lubricomp ZP001 PPE+PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Lubricomp ZP001 PPE+PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* ZP001 is a compound based on PPE+PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0082 cm/cm
0.0082 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
5 mm/min; ISO 527
Elongation at Yield 10.7 %
10.7 %
5 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Yield Strength 82.0 MPa
11900 psi
2 mm/min; ISO 178
Flexural Modulus 2.20 GPa
319 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af