SABIC Innovative Plastics LNP STAT-KON ME006 PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON ME006 PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 0.50 %
0.50 %
ASTM D638
Flexural Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 11.03 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.13 J/cm
3.99 ft-lb/in
ASTM D4812