Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Stat-kon DE006P PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Stat-kon DE006P PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* DE006P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.00040 - 0.00080 cm/cm
0.00040 - 0.00080 in/in
on tensile bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 166 MPa
24100 psi
5 mm/min; ISO 527
Elongation at Break 1.3 %
1.3 %
5 mm/min; ISO 527
Flexural Strength 190 MPa
27600 psi
2 mm/min; ISO 178
Flexural Modulus 18.0 GPa
2610 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 133 °C
271 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-1

@Thickness 1.60 mm
V-1

@Thickness 0.0630 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D 257