SABIC Innovative Plastics LNP THERMOCOMP BFL2200 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP BFL2200 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
design for black light frame application as high flow PC, V-2, high reflection grade.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 61.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
68.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 68.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
69.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2