SABIC Innovative Plastics Lexan® ML3260 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® ML3260 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.0 MPa
12000 psi
SABIC - Japan Method
Elongation at Break 10 %
10 %
SABIC - Japan Method
Flexural Strength 140 MPa
20300 psi
ASTM D790
Flexural Modulus 4.51 GPa
654 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 139 °C

@Thickness 3.20 mm
282 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
UL 94