SABIC Innovative Plastics Noryl GTX GTX6010 PPE+PA6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl GTX GTX6010 PPE+PA6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA6 based unfilled GTX. High impact.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D 792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0080 - 0.011 cm/cm

@Thickness 3.20 mm
0.0080 - 0.011 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.0 MPa
6240 psi
SABIC - Japan Method
Elongation at Break 150 %
150 %
SABIC - Japan Method
Flexural Strength 63.0 MPa
9140 psi
ASTM D 790
Flexural Modulus 1.76 GPa
255 ksi
ASTM D 790
Izod Impact, Notched 8.43 J/cm

@Temperature 23.0 °C
15.8 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 175 °C

@Thickness 3.20 mm
347 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Users viewing this material also viewed the following: