Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers GA-2190E-FR CLEAR PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GA-2190E-FR CLEAR PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Specialty clear, 60° C insulating compound designed for excellent clarity and sunlight resistance.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.26 g/cc
1.20 - 1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 95
90 - 95
ASTM D2240
Tensile Strength 16.2 MPa
2350 psi
ASTM D412
Elongation at Break 310 %
310 %
ASTM D412
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D746
Oxygen Index 27 %
27 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Weight Loss 0.022
7 days @ 100°C
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved