Material Notes:
Application: FR, UV and oil resistant PVC based compound with good low temperature properties.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.26 - 1.32 g/cc
1.26 - 1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
ASTM D2240
Tensile Strength 14.1 MPa
2050 psi
ASTM D412
14.24 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
2065 psi

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
16.64 MPa

@Treatment Temp. 100 °C,
Time 346000 sec
2413 psi

@Treatment Temp. 212 °F,
Time 96.0 hour
Aging in ASTM Oil #2
Elongation at Break 375 %
375 %
ASTM D412
243.75 %

@Treatment Temp. 100 °C,
Time 346000 sec
243.75 %

@Treatment Temp. 212 °F,
Time 96.0 hour
Aging in ASTM Oil #2
300 %

@Treatment Temp. 136 °C,
Time 605000 sec
300 %

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
Thermal Properties Metric English Comments
Brittleness Temperature -24.0 °C
-11.2 °F
ASTM D746
Oxygen Index 28 %
28 %
ASTM D2863
Users viewing this material also viewed the following: