Material Notes:
Description: PVC/Nitile alloy material designed for work boot applicationsInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 68
58 - 68
ASTM D2240
Tensile Strength 12.4 MPa
1800 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
Abrasion >= 284
>= 284
NBS; %; ASTM D1630
>= 136

@Load 1.02 kg,
Thickness 40000 mm
>= 136

@Load 2.25 lb,
Thickness 1570 in
mm<sup>3</sup>; DIN-53516
Descriptive Properties Value Comments
Rossflex >50000
@ -20°F, ASTM D1052
Slip Resistance 0.57
Wet, Mason tile, ASTM D1894
0.8
Dry, Mason tile, ASTM D1894
1.25
Wet, Varnished wood, ASTM D1894
1.32
Wet, Vinyl tile, ASTM D1894
1.59
Dry, Varnished wood, ASTM D1894
1.64
Dry, Vinyl tile, ASTM D1894
Stock Temperature 330-340°F