Material Notes:
Application: Non-migratory, non-contaminating, jacketing material designed to meet the requirements of Mil-C-17G Type 2a. This material has an operating temperature of 85° C to -45° C as per Mil C-17G type 2a specification.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.26 g/cc
1.20 - 1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 73
65 - 73
ASTM D2240
Tensile Strength 11.4 MPa
1650 psi
ASTM D412
11.97 MPa

@Treatment Temp. 113 °C,
Time 605000 sec
1736 psi

@Treatment Temp. 235 °F,
Time 168 hour
Air Oven aged
Elongation at Break 410 %
410 %
ASTM D412
348.5 %

@Treatment Temp. 113 °C,
Time 605000 sec
348.5 %

@Treatment Temp. 235 °F,
Time 168 hour
Air Oven aged
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746
Oxygen Index 26 %
26 %
ASTM D2863