S&E Specialty Polymers GM-3255 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GM-3255 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Non-toxic PVC material designed for molding applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.16 - 1.20 g/cc
1.16 - 1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 75
70 - 75
ASTM D2240
Tensile Strength 9.31 MPa
1350 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D412