S&E Specialty Polymers GTPO8102BA-H NATURAL PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GTPO8102BA-H NATURAL PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: High-flow flame retardant TPO compound for insulation and jacketing compound designed for ribbon cable applications. The flame retardant package incorporates non-PDBPO, PBB, PBDE flame-retardants, which is RoHS and WEEE compliant. The GTPO8102BA-H series of products is formulated to meet UL VW-1 testing, as well as CSA test C22-2 No. 0.6 flame test.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.17 - 1.23 g/cc
1.17 - 1.23 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 92 - 98
92 - 98
ASTM D2240
Tensile Strength >= 12.4 MPa
>= 1800 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Oxygen Index >= 26 %
>= 26 %
ASTM D2863
Descriptive Properties Value Comments
200% Modulus >6 lb-f
ASTM D638