Material Notes:
Application: 80°C, Low Smoke, Zero Halogen, Flame Retardant Polyethylene Compound for extrusion applications.    Specifically designed to withstand severe UV exposure while maintaining very good color stability.  Exhibits excellent processing characteristics at low temperature profile and lower motor load.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.28 - 1.32 g/cc
1.28 - 1.32 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 8.27 MPa
>= 1200 psi
ASTM D638
Elongation at Break >= 350 %
>= 350 %
ASTM D638
Thermal Properties Metric English Comments
Oxygen Index >= 27.5 %
>= 27.5 %
ASTM D2863