S&E Specialty Polymers TufFill™ GPP3003FD Natural Flame Retardant concentrate in Polyethylene

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer S&E Specialty Polymers
Trade Name TufFill™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFill™ GPP3003FD Natural Flame Retardant concentrate in Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame Retardant Concentrate in Polyethylene. GPP3003FD is PE based, flame retardant concentrate, with 1.61 g/cm3 Gravity, designed to impart flame resistance to polyolefin. Dependent upon let-down ratio in extrusion or molding grade resins, GPP3003FD can provide a range of V-2 to V-0 flammability UL-94 ratings. GPP3003FD performance in a specific resin system may be submitted to Underwriters Laboratories for confirmatory UL RecognitionInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.161 g/cc
1.161 g/cc
Thermal Properties Metric English Comments
Flammability, UL94 V-2 - V-0
V-2 - V-0