Material Notes:
Application: An extra flexible, expandable, PVC based compound suitable for injection molding applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 30.0

@Time 15.0 sec
30.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 5.52 MPa
801 psi
ASTM D412
Elongation at Break 200 %
200 %
ASTM D412
Processing Properties Metric English Comments
Processing Temperature 171 - 177 °C
340 - 350 °F
Suggested Stock