Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufLite™ GTPE-2001T TPE

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer S&E Specialty Polymers
Trade Name TufLite™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufLite™ GTPE-2001T TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A Thermoplastic Elastomer (TPE) designed for injection molding applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 49.0

@Time 15.0 sec
49.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 8.69 MPa
1260 psi
ASTM D412
Elongation at Break 355 %
355 %
ASTM D412
Users viewing this material also viewed the following: