Material Notes:
Application: A Flame Retardant Wire & Cable Jacketing Compound Rated at 75°C With Superior Low Temperature Properties and UV Resistance.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 78.0

@Time 15.0 sec
78.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 17.2 MPa
2490 psi
ASTM D412
14.104 MPa

@Temperature 100 °C,
Time 864000 sec
2045.6 psi

@Temperature 212 °F,
Time 240 hour
Oven Aging
Elongation at Break 300 %
300 %
ASTM D412
225 %

@Treatment Temp. 100 °C,
Time 864000 sec
225 %

@Treatment Temp. 212 °F,
Time 240 hour
Oven Aging
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746
Oxygen Index 26.0 %
26.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 168 - 174 °C
335 - 345 °F
Suggested Stock