S&E Specialty Polymers XP11-289A15 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers XP11-289A15 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PVC weatherable, integral colored, filled, high flow injection molding compound.Application: Body side molding which meets the Chrysler MSDC 543.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity <= 1.40 g/cc
<= 1.40 g/cc
ASTM D792, A
Mechanical Properties Metric English Comments
Hardness, Shore D 38 - 48

@Time 15.0 sec
38 - 48

@Time 0.00417 hour
ASTM D2240
Tensile Strength >= 17.5 MPa
>= 2540 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Descriptive Properties Value Comments
Accelerated Weathering <3.0 DE
after 2000 kj/m<sup>2</sup>, SAEJ2527
Cold Flex -30°C
MS-DC-543