SGL Carbon Group PANOX® LB C076 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer SGL Carbon Group
Trade Name PANOX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group PANOX® LB C076 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX is ideal for processing into yarns, woven fabrics, nonwovens and felts.Information provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.33 - 1.37 g/cc
0.0480 - 0.0495 lb/in³
Fiber Density
Water Absorption 9.0 %
9.0 %
Filament Diameter 21 µm
21 µm
Fiber Count 5.00 dtex
4.50 denier
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
Elongation at Break 19 - 27 %
19 - 27 %
Tenacity >= 0.150 N/tex
>= 1.70 g/denier
Descriptive Properties Value Comments
Crimps per cm 3.9
Mean Fiber Length, mm 76
Typical Finish Content, % 0.7