Material Notes:
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ASTM D2240
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength, Ultimate 43.1 MPa
6260 psi
ASTM D412
Tensile Strength, Yield 9.32 MPa

@Strain 100 %
1350 psi

@Strain 100 %
ASTM D412
18.6 MPa

@Strain 300 %
2700 psi

@Strain 300 %
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Resilience 39
39
by vertical rebound; ASTM D2632
Tear Strength 137 kN/m
784 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 30
30
H18 Wheel; 1000g load; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 110 °C
230 °F
ASTM D1525
Users viewing this material also viewed the following: