SPS Guang Zhou POFLEXâ„¢ EP8300 Cable Grade TPU

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer SPS Guang Zhou
Trade Name POFLEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou POFLEXâ„¢ EP8300 Cable Grade TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-halogen flame-retarded TPU material TPU POFLEXâ„¢ EP8300 is used to produce wire and cable. Halogen-free with good flammability and excellent mechanical property and heat resistance.Information Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 88

@Time 3.00 sec
88

@Time 0.000833 hour
ISO 868
Tensile Strength, Yield 7.50 MPa
1090 psi
100% Elongation; ASTM D412
9.50 MPa
1380 psi
300% Elongation; ASTM D412
26.0 MPa
3770 psi
ASTM D412
Elongation at Break 780 %
780 %
ASTM D412
Modulus of Elasticity 0.00700 GPa
1.02 ksi
50% Elongation; ASTM D412
Tear Strength 100 kN/m
571 pli
ASTM D624
Abrasion 30
30
loss; ASTM D1044
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
vertical burn
Oxygen Index 33 %
33 %
ASTM D2863
Descriptive Properties Value Comments
VW-1 Testing Passed
UI1581