Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

STAR Thermoplastic Alloys & Rubbers StarFlex® P 7350-1000 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarFlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarFlex® P 7350-1000 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: StarFlex P 7350-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades availableProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Viscosity 7700 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
7700 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 50

@Time 10.0 sec
50

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 4.31 MPa

@Time 7200 sec
625 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 880 %

@Time 7200 sec
880 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00108 GPa

@Time 7200 sec
0.156 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 21.0 kN/m
120 pli
ASTM D624
Descriptive Properties Value Comments
Color Natural
Users viewing this material also viewed the following: