Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

STAR Thermoplastic Alloys & Rubbers StarFlex® P 7390-9000 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarFlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarFlex® P 7390-9000 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: StarFlex P 7390-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Viscosity 11300 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
11300 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 90

@Time 10.0 sec
90

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 8.239 MPa

@Time 7200 sec
1195 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 770 %

@Time 7200 sec
770 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00491 GPa

@Time 7200 sec
0.712 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 38.6 kN/m
220 pli
ASTM D624
Descriptive Properties Value Comments
Color Black