STAR Thermoplastic Alloys & Rubbers StarTUFF TF 55-HR-1 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarTUFF
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarTUFF TF 55-HR-1 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: StarTUFF TF 55-HR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Viscosity 13900 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
13900 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 55

@Time 10.0 sec
55

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 7.45 MPa

@Time 7200 sec
1080 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 750 %

@Time 7200 sec
750 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00153 GPa

@Time 7200 sec
0.222 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 31.2 kN/m
178 pli
ASTM D624