Saint-Gobain COHRlastic® R10490 Medium Fluorosilicone Sponge Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name COHRlastic®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain COHRlastic® R10490 Medium Fluorosilicone Sponge Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R10490 fluorosilicone sponge rubber can be used as a gasket where it is necessary to contain fluids that would degrade normal silicone sponge and solid materials (special order basis). Specification Notes: Meets Specifications: MIL-R-6130 Type II, Grade A. All data based on a 0.0625 inch test sample.(Other thicknesses available.)Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.554 g/cc
0.0200 lb/in³
ASTM D3574
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D1056
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.24 MPa
180 psi
ASTM D412
Elongation at Break 125 %
125 %
ASTM D412
Compressive Strength 0.103 MPa

@Temperature 23.0 °C
15.0 psi

@Temperature 73.4 °F
ASTM D1056
Compression Set 25 %
25 %
ASTM D1056
Thermal Properties Metric English Comments
CTE, linear 324 µm/m-°C

@Temperature 20.0 - 177 °C
180 µin/in-°F

@Temperature 68.0 - 350 °F
Specific Heat Capacity 1.26 J/g-°C
0.300 BTU/lb-°F
Thermal Conductivity 0.108 W/m-K
0.750 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 5.71 kV/mm
145 kV/in
Descriptive Properties Value Comments
Color Blue