Saint-Gobain Chemlam® 6 Value Industrial Laminate

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Chemlam®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Chemlam® 6 Value Industrial Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass reinforcements. Chemfab® laminates outperform traditional PTFE_coated products of similar weight and thickness. FEATURES: PTFE cast barrier film surface, crack and pinhole free: Outperforms simple PTFE-coated materials; long-lasting release properties make cleaning easier; low wicking properties extend useful life.Uniform film thickness over entire surface: Lamination eliminates the possibility of thin spots found in coated materials, which often lead to their premature failure.High temperature fabrics: Designed for thermal cycling and harsh chemical applications, including cooking and plastic processing.FDA Compliant: Suitable for use in direct food contact applications under the applicable requirements of 21CFR177.1550. All data based on a 0.0058 inch test sample. Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 2.025 g/cc
2.025 g/cc
Woven Density
Mechanical Properties Metric English Comments
Tear Strength Test 4.5
4.5
Lbs./In. Propagation Tear Strength in fill/transverse direction
5.0
5.0
Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 21.0 kN/m
120 pli
Warp/Longitudinal direction
21.0 kN/m
120 pli
Fill/Transverse direction
Descriptive Properties Value Comments
Color Brown/Brown
Weight (oz/yd^2) 8.8